Addcomp PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name PRIEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypropylene.Examples: Compatibilising short-and long glass fibers and PP applications such as automotive applications (instrument panel carrier, front-end, door modules, etc.) and Wood filled polymer composites.Mode of action and advantages: PRIEX® 20093 is a polypropylene, grafted with a high content of maleic anhydride. The grafted maleic anhydride introduces polarity to the polymer achieving compatibility between polyolefins and more polar polymers like EVOH.Advantages: Excellent mechanical properties, good cost / performance; Ultra low smell, low VOC and emissions; Excellent coupling agent for short and long glass filled polyolefins providing enhanced physical, mechanical and thermal properties; Excellent coupling agent for natural fiber reinforced polymer composites or wood flour reinforced polymer composites; Free flowing pellets; and Safe and easy handling.Food contact: PRIEX® 20093 composition meets the requirements of Commission Directive 2002/72/EC and further amendments.Information provided by Addcomp Polymer Additive Solutions
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183-3
Viscosity Measurement 0.070 - 0.080
0.070 - 0.080
[l/g], Intrinsic viscosity; ISO 1628
Oxidative Induction Time (OIT) >= 20 min

@Temperature 190 °C
>= 20 min

@Temperature 374 °F
ISO 11357-6
Melt Flow 9.0 - 13 g/10 min

@Load 0.325 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 0.716 lb,
Temperature 374 °F
die 8/2; ISO 1133
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
ISO 11357-3
Processing Properties Metric English Comments
Processing Temperature <= 280 °C
<= 536 °F
Descriptive Properties Value Comments
Appearance White or slightly yellow granules
Free Aleic Anhydride <250 mg/kg
Solvay method
Grafted Maleic Anhydride 0.17-0.21%
Solvay method