Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Ultimate 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 12.5 %
12.5 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 5.20 GPa
754 ksi
ASTM D790
Compressive Yield Strength 186 MPa
27000 psi
ASTM D695
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ASTM D648
Flammability, UL94 HB
HB