Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 69
69
ASTM D785
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Ultimate 48.3 MPa
7010 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Gardner Impact 0.500 J
0.369 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Flammability, UL94 HB
HB