Adell ZR-17 33% Glass Reinforced Nylon/Olefin Alloy

Category Polymer , Thermoplastic , Nylon
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell ZR-17 33% Glass Reinforced Nylon/Olefin Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
1.12 J/cm

@Temperature -40.0 °C
2.10 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
5.13 J/cm

@Temperature -40.0 °C
9.60 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Gardner Impact 1.20 J
0.885 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F