Material Notes:
60°C rated jacket compound.
Mechanical Properties Metric English Comments
Tensile Strength 18.6 MPa
2700 psi
Elongation at Break 230 %
230 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -15.0 °C
5.00 °F
Oxygen Index 40 %
40 %