Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE HMW 1000950 features good melt strength, excellent stress cracking resistance, good rigidity, and excellent impact strength. Applications include agricultural chemical tanks, pallets, and large formed and blow molded parts.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 600 hour
>= 600 hour
Condition A, F50
>= 600 hour
>= 600 hour
Condition B, F50
Melt Index of Compound 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
50 mm/min, Type IV; ASTM D638
Elongation at Break >= 600 %
>= 600 %
50 mm/min, Type IV; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.6 °C
<= -131 °F
ASTM D746
Users viewing this material also viewed the following: