Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.949 - 0.953 g/cc | 0.0343 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6752E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E904 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsInformation provided by Formosa Plastics Corporation, USA. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E905 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Density | 0.949 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GP 9452 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | |
JPJ Technologies 7600M HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L4907 High Density Polyethylene ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5040TC High Density Polyethylene ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r.. |
|||
Density | 0.949 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 9450 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total 49080 UV HDPE blow molding FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E925 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E925 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9505H High Density Polyethylene This gas phase, high molecular weight, hexene copolymer with antistatic agent is tailored for lightweight blow molded containers that:Require outstanding ESCRRequire excellent impact resistanceAre d.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | natural resin; ASTM D792 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 621 HD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid HDPEInformation provided by Fainplast Compounds.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerCustomer Benefits: A high performance copolymer that can measure up to the most demanding application. Specifically formulated to provide toughness and durabil.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
Dow UNIPOL™ DGDA-5110 Polyolefin DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer HDPE HMW 1000950 features good melt strength, excellent stress cracking resistance, good rigidity, and excellent impact strength. Applications include agricultural chemical tanks, pallets, and large.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924F Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Film Applications Formolene® E924F is a “low gel” high molecular weight grade of HDPE designed for high dart impact strength and.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |