Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Polymers API 650-21 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer American Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers API 650-21 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applications: Widely used in appliance housings, toys, bathroom accessories and displays.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 45
45
ASTM D785
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 48 %
48 %
ASTM D638
Tensile Modulus 1.99 GPa
288 ksi
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm

@Thickness 3.17 mm
2.70 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Annealed; ASTM D648
Vicat Softening Point 88.9 °C
192 °F
ASTM D1525
Users viewing this material also viewed the following: