Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 89.0 °C | 192 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Network Polymers NPS 90-0827 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 88.9 °C | 192 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 4241 High Impact Polystyrene
(discontinued **) DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | |
Ineos ABS NOVODUR® L3FR ABS, Injection Grade
(discontinued **) Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | |
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ISO 306B |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | 50°C/h; 10N; 10x10x4mm; ISO 306/A50 |
SYNTHOS Krasten® 137 General Purpose Polystyrene Easy flow. Examples of Application:Injection moulding – cups and containers for the food industry, medical devices, drawing templates.Extrusion – coextrusion, high gloss surface.Synthos wa.. |
|||
Vicat Softening Point | 89.0 °C @Load 5.10 kg |
192 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS ESCRimo HIPS Styrolution PS ESCRimo is a high impact polystyrene grade with an improved stress cracking resistance compared to conventional high impact polystyreneHigh ESCR resistanceDeep draw thermoformingUL 94.. |
|||
Vicat Softening Point | 88.9 °C | 192 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRF 2704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance; Good Processability Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Te.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | B (50N); ISO 306 |
Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat sta.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | 50N-50°C per hour; ISO 306 |
Total PPH 9069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9069 is homopolymer.ApplicationATOFINA Polypropylene PPH 9069 is intended for applications in non-wovens. It is also suitable for extrusion of bulk continuous filament (BC.. |
|||
Vicat Softening Point | 88.9 °C | 192 °F | ASTM D1525 |
American Polymers API 650-21 Polystyrene API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applicat.. |
|||
Vicat Softening Point | 88.9 °C | 192 °F | ASTM D1525 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Braskem PB 682 LDPE Blow Molding Polyethylene Description: PB682 is a low density polyethylene (LDPE), produced under high pressure technology. The end products molded with this resin present good dimensional stability and high flexibility.Appl.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | |
BASF Polystyrol® 165 H Polystyrene (Europe) High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | |
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Huntsman PE2050 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewares and toys.FDA Notes: Conforms to.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ASTM D1525 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | ISO 306A |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | 50°C/h; 10N; 10x10x4mm; ISO 306/A50 |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |
|||
Vicat Softening Point | 89.0 °C | 192 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |