Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Americas Styrenics LLC
Trade Name STYRON A-TECH®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration AccessoriesInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 1.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength at Break 29.0 MPa
4200 psi
ASTM D638
Tensile Strength 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Tensile Modulus 1.38 GPa
200 ksi
ASTM D638
Flexural Strength 31.7 MPa
4600 psi
ASTM D790
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
compression molded; ASTM D256
0.908 J/cm
1.70 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525