Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.35 g/cc Green Density

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.35 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement in corrosion resistance, while other properties are comparable to the conventional counterparts.Mechanical property data below is from samples lubricated with 1% Acrawax C and pressed at 40 tsi. Green strength 1000 ksi. Specimens were delubricated in air for 20 min. at 950°F (510°C), then sintered in dissociated ammonia for 30 min. at 2100°F (1149°C) and cooled in the water jacketed furnace cooling zone. Dimensional change from die size -0.20%.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Density 6.41 g/cc
0.232 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 50
50
Tensile Strength, Ultimate 290 MPa
42100 psi
Tensile Strength, Yield 230 MPa
33400 psi
Elongation at Break 4.1 %
4.1 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 18 %
18 %
Copper, Cu 0.80 %
0.80 %
Iron, Fe 67 %
67 %
as balance
Manganese, Mn 0.20 %
0.20 %
Nickel, Ni 11 %
11 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.80 %
0.80 %
Sulfur, S 0.20 %
0.20 %
Tin, Sn 2.0 %
2.0 %