Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape  (disco

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.0 %
1.0 %
Arlon SQA-TMS-016
Thickness 25.4 microns
1.00 mil
Polyester Film, Interleave
762 microns
30.0 mil
Overall; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.93 MPa
1150 psi
Silicone Property; ASTM D412
Elongation at Break 430 %
430 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 0.578 kN/m
3.30 pli
[ppiw], Government Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.0 kV/mm
610 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following: