Arlon LW301CxxFR-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon LW301CxxFR-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length in yards.Design/Construction: Interleave: Polyethylene
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
762 microns
30.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 4.21 MPa
610 psi
Silicone Property; ASTM D412
Elongation at Break 500 %
500 %
Silicone Property; ASTM D412
Peel Strength 0.561 kN/m
3.20 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Flammability Test 0.60
0.60
[in], Char Length; FAR 25.853 App. F, P.1,.Aii
4.4
4.4
[sec], Flame and Glow; FAR 25.853 App. F, P.1,.Aii
Electrical Properties Metric English Comments
Dielectric Strength 18.3 kV/mm
465 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Brown