Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Leona® 1300G Polyamide 66 Resin, Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer Asahi Kasei
Trade Name Leona®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Leona® 1300G Polyamide 66 Resin, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive: Radiator Tanks, Fuel Injectors, ABS Sensors, Engine Mounts Electrical and Industrial: Heater Tanks, Office Furniture, Small EnginesInformation provided by Asahi Kasei
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
23°C
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
Wet
190 MPa
27600 psi
Dry
Elongation at Break 3.0 %
3.0 %
Dry
5.0 %
5.0 %
Wet
Flexural Modulus 6.80 GPa
986 ksi
Wet
9.00 GPa
1310 ksi
Dry
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
Dry
1.60 J/cm²
7.61 ft-lb/in²
Wet
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 265 °C
509 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved