Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Tenac®-C 5520 Copolymer Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Asahi Kasei
Trade Name Tenac®-C
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Tenac®-C 5520 Copolymer Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Similar to TENAC®-C 4520 but with higher flow and minimized mold deposit.Information provided by Asahi Kasei Corporation.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Linear Mold Shrinkage 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
Asahi Kasei Method
Melt Flow 15 g/10 min
15 g/10 min
ISO 1133 D
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.0 MPa
9570 psi
ISO 527 - 1 & - 2
Elongation at Break 50 %
50 %
ISO 527 - 1 & - 2
Tensile Modulus 2.85 GPa
413 ksi
ISO 527 - 1 & - 2
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 / 1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 156 °C
313 °F
ISO 75 -1 & -2 flat
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75 -1 & -2 flat
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: