Asahi Kasei Thermofil N-40MF-1600 40% Mineral Filled, Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil N-40MF-1600 40% Mineral Filled, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm
9.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 43.2 µm/m-°C

@Temperature 20.0 °C
24.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
425 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648