Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1200 A UV White 205 Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal 25% Glass Fiber Reinforced Copolymer AcetalInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
PTS PPE/Nylon Alloy 10% Glass Filled Information provided by PTS LLC. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-10CF/15T-2S Acetal-Copolymer, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(disco Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled 20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | .01% permanent set |
Meehanite GE-30 Flake Graphite Cast Iron Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Electrablend® PA6/PC Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionTPCI# 9586102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 HS L MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantHeat Stabilized and LubricatedTPCI# 7018102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated Features: Good chemical resistanceFast cycleDurableLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100M2HS (Dry) Nylon 66, Lubricated, Heat Stabilized Features: Good chemical resistanceFast cycleDurableHeat stabilizedLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-25GF-10MN/000 NATURAL Acetal-Copolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |