Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.59 GPa
520 ksi
ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
6.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 166 °C
330 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Users viewing this material also viewed the following: