Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermylene® P6-40FG-0874 40% Glass Fiber Reinforced, Heat and UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P6-40FG-0874 40% Glass Fiber Reinforced, Heat and UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Melt Flow 6.5 g/10 min
6.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 96.5 MPa
14000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 7.31 GPa
1060 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812