Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® PBT 130, 50% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® PBT 130, 50% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 50% glass reinforced PBT designed for maximum rigidity of engineered parts.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 152 MPa
22000 psi
ATSM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ASTM D3418
Maximum Service Temperature, Air 120 °C
248 °F
Long term
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648