Polymer Property : Tensile Strength = 2610 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 18.0 MPa
2610 psi
ISO 527
S&E Specialty Polymers TufFill™ 5003UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..
Tensile Strength 18.0 MPa
2610 psi
ISO 527
S&E Specialty Polymers TufFill™ 5004UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..
Tensile Strength >= 18.0 MPa
>= 2610 psi
DIN 53504
NEXA® PFX8010 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
Tensile Strength >= 18.0 MPa
>= 2610 psi
DIN 53504
NEXA® PFX8012 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
Tensile Strength >= 18.0 MPa
>= 2610 psi
DIN 53504
NEXA® PFX8034 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
Tensile Strength 18.0 MPa
2610 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound
PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi..
Tensile Strength 18.0 MPa
2610 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa..
Tensile Strength 18.0 MPa
2610 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data)
Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The..
Tensile Strength 18.0 MPa
2610 psi
ASTM D412
GRECO ISOTHANE 1680AE Polyether TPU Resin
ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf..
Tensile Strength 18.0 - 23.0 MPa
2610 - 3340 psi
ASTM D4894
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic
Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon.
Tensile Strength 18.0 - 23.0 MPa
2610 - 3340 psi
ASTM D4894
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite
Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon.
Tensile Strength 18.0 MPa
2610 psi
ISO 527
MRC Polymers MAXTELâ„¢ 620-BK Polypropylene Copolymer
• For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc.
Tensile Strength 18.0 MPa
2610 psi
DIN 53504
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
Peroxide Cured
Tensile Strength 18.0 MPa
2610 psi
ASTM D638
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls
DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig..
Tensile Strength >= 18.0 MPa
>= 2610 psi
ISO 37
Austin Novel Materials Texalan® 265A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Strength >= 18.0 MPa
>= 2610 psi
ISO 37
Austin Novel Materials Texalan® 765A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Strength >= 18.0 MPa
>= 2610 psi
ISO 37
Austin Novel Materials Texalan® 570A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Strength 18.0 MPa

@Strain 100 %
2610 psi

@Strain 100 %
ISO 37
BASF Elastollan S 60 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength >= 18.0 MPa
>= 2610 psi
extruded; ASTM D1708
Guarniflon PTFE G300 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..