Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 570A Polyether-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 570A Polyether-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.04 - 1.08 g/cc
0.0376 - 0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 73
67 - 73
ISO 7619
Tensile Strength >= 18.0 MPa
>= 2610 psi
ISO 37
Tensile Stress >= 2.00 MPa

@Strain 100 %
>= 290 psi

@Strain 100 %
ISO 37
>= 3.50 MPa

@Strain 300 %
>= 508 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 700 %
>= 700 %
ISO 37
Tear Strength >= 50.0 kN/m
>= 285 pli
ISO 34
K Factor (Wear Factor) <= 90
<= 90
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 30 %

@Temperature 70.0 °C
<= 30 %

@Temperature 158 °F
ISO 815
Users viewing this material also viewed the following: