Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D792 |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina 802-06/795-CRM Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina 837-35/1-A-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina 937-48/1-CY-IS-BZ Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 18/89-FC-LMP Gray Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina E 845-35/2-CRM Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.401 - 1.42 g/cc | 1.401 - 1.42 g/cc | |
Dow UVI-6976 Photoinitiator UVI-6976 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6976 photoinitiator is used to UV-cure CYRACURE™ cycloaliphati.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AK-050380 PVC Description: Compuestos Dominicanos, S.A. manufactures PVC compounds for the production of high quality electrical wire and cable with excellent insulation properties and smooth finish. Polycom prod.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AK-051090 PVC Compound Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 1131-57D Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 12792 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 12802 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacket recommended for 75C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 14890 Wire & Cable Flexible PVC General purpose UL approved 720 hour sunlight resistant jacket suitable for a maximum 80°C temperature rating at a 1/32" wall. Recommended for UF-B and NM-B constructions and also RG59 coaxial cab.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 16902 Wire & Cable Flexible PVC Non-lead stabilized, 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 17870 Wire & Cable Flexible PVC TW, THW insulation compound. Oil II rated. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 22902 Coax & Telecom Flexible PVC Non-lead stabilized riser jacket recommended over PVC and FRHDPE primaries. Maximum service temperature rating of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 38951 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8758 Moldings & Extrusions Flexible PVC A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8850 Moldings & Extrusions Flexible PVC General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8880 Moldings & Extrusions Flexible PVC General purpose non-lead stabilized extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8910 Moldings & Extrusions Flexible PVC Extrusion compound especially formulated for extruded T-moldings, tubings, and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall EX1063 Coax & Telecom Flexible PVC Non-lead stabilized, fiber optic compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 12791 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties and 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall .. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 1055 Wire & Cable Flexible PVC NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 4750 Flexible PVC General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.42 g/cc | 1.36 - 1.42 g/cc | ASTM D 792 |
Karina 837-10/37-A-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AU-050695 PVC Compound Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d.. |