| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | Axiall |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Axiall 18660 Moldings & Extrusions Flexible PVC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 63 - 69 | 63 - 69 | delayed; ASTM D-2240 |
| Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D-638 |
| Elongation at Yield | 350 % | 350 % | ASTM D-638 |
| 100% Modulus | 0.00362 GPa | 0.525 ksi | ASTM D-638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D-746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 185 °C | 365 °F |