Polymer Property : Tensile Strength, Yield = 1400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Polymax® Maxelast® P3675 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 9.65 MPa
1400 psi
chs 20 in/min; ASTM D412
Network Polymers Softflex® 7210 Black
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 9.65 MPa
1400 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Strength, Yield 9.65 MPa
1400 psi
molding; ASTM D638
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma..
Tensile Strength, Yield 9.65 MPa
1400 psi
Molded; ASTM D638
LyondellBasell Petrothene® NA942094 Low Density Polyethylene
ApplicationsPETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and c..
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D638
Global TPE-LS70A Elastomer Grade
Data provided by Global Polymers Corporation.
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D 638
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'..
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex APEX® 90-A472R-55-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-..
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex Flexalloy® 9900-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex MONPRENE® MP 2860E Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex MONPRENE® MP 2860M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D412
Teknor Apex APEX® 3210-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 9.65 MPa
1400 psi
at 300%; ASTM D412
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation
Tensile Strength, Yield 9.65 MPa
1400 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D..
Tensile Strength, Yield 9.65 MPa
1400 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D-638
Axiall 6570 Moldings & Extrusions Flexible PVC
General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D-638
Axiall 8757 Moldings & Extrusions Flexible PVC
Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 9.65 MPa
1400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 9.65 MPa
1400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 9.65 MPa

@Strain 300 %
1400 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 39-020 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerWeatherable GradeApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Extrusion and Moldin..
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D-638
Axiall 18660 Moldings & Extrusions Flexible PVC
Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.