Axiall 7450 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7450 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical ResistanceEase of Processing-Low Die SwellInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D-785
Hardness, Shore D 75
75
ASTM D-2240
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Tensile Modulus 2.45 GPa
355 ksi
ASTM D-638
Flexural Strength 81.4 MPa
11800 psi
ASTM D-790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D-790
Izod Impact, Notched 4.27 J/cm

@Thickness 6.35 mm
8.00 ft-lb/in

@Thickness 0.250 in
ASTM D-256
9.61 J/cm

@Thickness 3.17 mm
18.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 168 kJ/m²
80.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 133 J/cm
0.250 ft-lb/mil
H.25 Tup, Method A; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
154 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Cell Classification 14423223
ASTM D-4216