Material Notes:
Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of ProcessingUL RatingInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.81 GPa
408 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.45 GPa
356 ksi
ASTM D-790
Izod Impact, Notched 2.67 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
5.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
13.9 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
26.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 172 kJ/m²
82.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 178 J/cm
0.333 ft-lb/mil
ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
154 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Tested in Georgia Gulf labs
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Cell Classification 1-434-33-00
ASTM D-4216
Users viewing this material also viewed the following: