Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2.81 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.81 GPa
408 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding 87546 Polyvinyl Chloride, Rigid (PVC, Rigid)
Provisional Data SheetInformation provided by PolyOne
Tensile Modulus 2.81 GPa

@Thickness 6.40 mm
408 ksi

@Thickness 0.252 in
ASTM D 638
SABIC Innovative Plastics Lexan® FL3000 PC
Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp..
Tensile Modulus 2.81 GPa
408 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.81 GPa

@Thickness 6.40 mm
408 ksi

@Thickness 0.252 in
ASTM D 638
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific)
Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci..
Tensile Modulus 2.81 GPa

@Temperature -18.0 °C
408 ksi

@Temperature -0.400 °F
1-mm/min; ISO 527
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade
Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components.
Tensile Modulus 2.81 GPa
408 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.81 GPa
408 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.81 GPa
408 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 2.81 GPa
408 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific)
LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*..
Tensile Modulus 2.81 GPa
408 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS
high gloss Noryl
Tensile Modulus 2.81 GPa
408 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Tensile Modulus 2.81 GPa
408 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Tensile Modulus 2.81 GPa
408 ksi
ASTM D-638
Axiall 7456 Rigid PVC, Extrusion
Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of Proces..
Copyright © lookpolymers.com All Rights Reserved