Material Notes:
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connectors etc. in household appliance.Information provided by BASF
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Melt Flow 258 g/10 min

@Load 5.00 kg,
Temperature 275 °C
258 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50 mm/min; ISO 527-1/-2
Elongation at Yield 10 %
10 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity 1.10 GPa
160 ksi
ISO 527-1/-2
Flexural Strength 40.0 MPa
5800 psi
at max force; ISO 178
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
DIN 53765
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
350 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Injection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection-molding
Descriptive Properties Value Comments
Color BK 23079
Commercial Status Europe
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved