Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BP Amoco Acclear® 6219 Homopolymer Polypropylene, High Clarity Grade  (discontinued **)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BP Amoco Acclear® 6219 Homopolymer Polypropylene, High Clarity Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Suggested fabrication methods: Sheet extrusion; ThermoformingFeatures: High clarity, High heat resistance, Good melt strength/flow balanceTypical applications: Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790A
Izod Impact, Notched 0.320 J/cm

@Diameter 3.17 mm
0.599 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ASTM D648
Optical Properties Metric English Comments
Haze 23 %

@Thickness 1.27 mm
23 %

@Thickness 0.0500 in
plaque; ASTM D1003
Transmission, Visible 90 %
90 %
clear; thickness not quantified