Bales Mold Service QQ-N-290 Sulfamate Nickel Mold Coating

Category Metal , Nonferrous Metal , Nickel Alloy , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Bales Mold Service
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bales Mold Service QQ-N-290 Sulfamate Nickel Mold Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Selective plating for dimensional correction is a typical application for Sulfamate Nickel because of it's ability to deposit up to .250 with less inclusions and porosity than most electrolytic deposits. This is an excellent choice for deposits in excess of .015-.020 thick.Information provided by Bales Molding Service Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 40
40
Coefficient of Friction <= 0.45
<= 0.45
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
Applied Temperature