Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 60.0 °C | 140 °F | Curing Agent Temperature |
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Processing Temperature | 60.0 °C | 140 °F | Chill Roll |
LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade ALATHON H6012 is medium molecular weight high density polyethylene homopolymer for use in cast film applications. Typical applications for this resin include extrusion coating, blends with LDPE and .. |
|||
Processing Temperature | 60.0 - 150 °C | 140 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin 78 NanoCoating Transparent, scratch-resistant coating also for plastics with good resistance against dissolvents.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials G2020520D1 Gold Metallo-Organic Ink This is a screen printing ink designed to act as a working electrode when fired onto alumina substrates. This unique MO formulation gives a fired thickness in the order of 0.2 to 0.3 microns. This.. |
|||
Processing Temperature | >= 60.0 °C | >= 140 °F | Activation Temperature; EN-12961 |
Lubrizol Advanced Materials Pearlstick® 48-60/30 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/30 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |
|||
Processing Temperature | 60.0 °C | 140 °F | EN-12961 |
Lubrizol Advanced Materials Pearlstick® D40-70/08 Linear Thermoplastic Polyurethane Pearlstick D40-70/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. S.. |
|||
Processing Temperature | 60.0 °C | 140 °F | non show side |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Processing Temperature | 60.0 °C | 140 °F | Applied Temperature |
Bales Mold Service QQ-N-290 Sulfamate Nickel Mold Coating Selective plating for dimensional correction is a typical application for Sulfamate Nickel because of it's ability to deposit up to .250 with less inclusions and porosity than most electrolytic .. |
|||
Processing Temperature | 60.0 - 240 °C | 140 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 60.0 - 120 °C | 140 - 248 °F | Barrel temperature |
Azoty Tarnow™ TARNOFORM 200 HI4 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Processing Temperature | 60.0 °C | 140 °F | hopper drying; 4h |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Processing Temperature | 60.0 °C | 140 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 46-73/27 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |