Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP4022 is a PP homopolymer designed for oriented film applications. It offers good clarity and optical properties. This resin meets FDA standards for food contact applications.Applications: Oriented film, monofilaments, split fibers.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D-785
Tensile Strength, Yield 33.8 MPa
4900 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 200 %
200 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 10 %
10 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.34 GPa
194 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM D648
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
International