Barlog Plastics KEBABLEND W/H 23.10.1 PBT functional compound, high density

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Barlog Plastics
Trade Name KEBABLEND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBABLEND W/H 23.10.1 PBT functional compound, high density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT mod.Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.0 MPa
5220 psi
ISO 527-1
Elongation at Break 10 %
10 %
ISO 527-1
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Resin Type PBT mod.