Borealis BD950MO Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BD950MO Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability, high melt strength and extremely low tendency to stress whitening. This grade uses Borealis Nucleation Technology (BNT) to increase productivity by cycle time reduction. As with all BNT grades, products exhibit excellent dimensional consistency with different colorants. In addition, this grade provides excellent creep resistance and optimum stiffness-impact balance. This polymer contains slip and antistatic additives to ensure good demolding properties, low dust attraction and low friction coefficient which meets the industry standards for closure opening torques. Applications: caps and closures for beverage food and industrial packaging.Information provided by Borealis AG
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ISO 2039-2
Tensile Strength, Yield 27.0 MPa
3920 psi
50mm/min; ISO 527-2
Elongation at Yield 4.5 %
4.5 %
50mm/min; ISO 527-2
Tensile Modulus 1.50 GPa
218 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 15.0 J

@Temperature -20.0 °C
11.1 ft-lb

@Temperature -4.00 °F
ISO 6603-2
20.0 J

@Temperature 0.000 °C
14.8 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity highest possible