Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 22.2 - 30.0 °C | 72.0 - 86.0 °F | |
Northstar Polymers MPP-W43C Polyurethane Gel MPP-W43C is a polyurethane gel formulation specifically designed for padding and cushioning applications that require Shore Durometer OOO scale hardness materials. With this material, a user can ob.. |
|||
Mold Temperature | 22.2 - 30.0 °C | 72.0 - 86.0 °F | |
Northstar Polymers GK-22 Polyurethane Gel for Adhesion Pad Applications GK-22 is a polyurethane gel formulation designed to make soft sticky polyurethane gel for pressure-sensitive-adhesive type products. This 2-part cast urethane system can be manually processed easi.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HG313MO Polypropylene HG313MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grad is designed for high-speed inject.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HG385MO Polypropylene HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polyprop.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HG430MO Polypropylene HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HJ325MO Polypropylene HJ325MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. is designed fo.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis Bormod™ BE961MO Polypropylene for Injection Molding Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1000 Polymer, Natural Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar EN052 Polyester Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar EN063 Polyester Eastar Polyester EN063 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Eastar Polyester EN063 is a homopolymer .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® MX 1205 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arke.. |
|||
Mold Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
LATI Latistat 48/9900-03 EVA Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |