Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BC650MO Polypropylene Copolymer BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BE170MO Polypropylene Copolymer BE170MO is a heterophasic copolymer. This grade is characterized by high impact strength, high stiffness and good flow properties. This grade contains additives providing low taste and odor as well.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BG373MO Polypropylene Copolymer BG373MO is a heterophasic copolymer. Products molded with this grade exhibit excellent antistatic performance and very good mould release. Electrostatic charge is |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BH980MO Polypropylene Copolymer BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis HG385MO Polypropylene HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polyprop.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis HH315MO Polypropylene HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis HJ320MO Polypropylene HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is .. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis HJ325MO Polypropylene HJ325MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. is designed fo.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis RG460MO Polypropylene, Transparent Random Copolymer RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis RJ370MO Polypropylene, Transparent Random Copolymer RJ370MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate. It is designed for high-speed injection molding and contains nucleating and demoldin.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis RJ470MO Polypropylene, Transparent Random Copolymer RJ470MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate and is designed for high-speed injection molding and contains nucleating and demolding.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Hold Pressure | 25.0 - 50.0 MPa | 3630 - 7250 psi | Injection Molding |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Hold Pressure | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Borealis RF365MO Polypropylene Applications: closures, thin wall containers, and excellent transparency.Information provided by Borealis AG |