Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Borealis
Trade Name BorPEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. Crosslinked pipes made from BorPEX HE2556 are recommended for drinking water and industrial applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Base Resin; ISO 1183
0.966 g/cc
0.0349 lb/in³
Compound; ISO 1183
Carbon Black Loading 2.2 %
2.2 %
ASTM D1603
High Load Melt Index 6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
50 Minutes; EN 728