Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | >= 210 °C | >= 410 °F | pending UL RTI |
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | UL temperature Index 200/220°C (400/430°F) |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Maximum Service Temperature, Air | 210 °C @Time 5.40e+6 sec |
410 °F @Time 1500 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | < 50 h; IEC 60216/T1 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Maximum Service Temperature, Air | 210 - 230 °C | 410 - 446 °F | Softening Range |
Huntsman DT 3368 Matting Agent Color: Off-whiteComments/Applications: Reactive matting agent for very low gloss epoxy and epoxy/polyester hybrid powder formulations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemica.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Greene Tweed CHEMRAZ® 543 Perfluoroelastomer Chemraz® 543 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contamination is required. It offers excellent performan.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Heat Resistance; DIN 53772 |
Karina 4000/35-IE MBPEBD Green Color Concentrate Color concentrate recommended for polyolefin applications and 2% minimum adding.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Heat Resistance; DIN 53772 |
Karina E 3600/004-IE MBU Brown Color Concentrate Brown pigment concentrate recommended for polyolefin, polyolefinic compound, and general PVC compound. Usage 1% minimum. Organic and inorganic.Information provided by Karina Indústria e Comé.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Greene Tweed CHEMRAZ® 570 Perfluoroelastomer Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent perfor.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | 50 Minutes; EN 728 |
Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstand.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | 50 Minutes; EN 728 |
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Up to 3 hours |
Master Bond MB516 Hot Melt Adhesive Compound Master Bond Polymer System MB516 is a pelletized extra tough, high strength, low viscosity polyamide resin composition for the hot melt bonding of plastics, metals and wood. It features excellent th.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Elisto THERMOSTAR® 4000 Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Epoxyset Epoxibond EB-315 Low Expansion Epoxy Adhesive EB-315 is a highly filled, heat curing, high temperature resistant epoxy adhesive. Due to its low coefficient of thermal expansion and outgassing, it can be used for bonding and sealing in critical .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Elisto THERMOSTAR® XPS Mold Insulation Material Lateral insulationInformation provided by elisto |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4300 G4 High Speed Unc. 20% Glass Filled PBT Ultradur B 4300 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 210 °C @Time 4.32e+6 sec |
410 °F @Time 1200 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |