Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed LE6609-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.Bormed LE6609-PH can be used in "blow-fill and seal" machines for the production of ampoules and bottles. The product can also be used for pharmaceutical products manufactured with other conversion techniques such as injection molding and film blowing. LE6609-PH will withstand heating up to 110°C and therefore units made from this product may be steam treated to max 110°C.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868
Tensile Strength, Yield 14.0 MPa
2030 psi
50 mm/min; ISO 527-2
Tensile Modulus 0.400 GPa
58.0 ksi
At 1 mm/min; ISO 527-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C
129 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 165 - 200 °C
329 - 392 °F