Borealis Borstar® ME3446 Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black MD Pipe for Natural Gas

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Borstar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borstar® ME3446 Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black MD Pipe for Natural Gas.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borstar 3446 is a bimodal, cadmium free, medium density polyethylene compound designed for coextrusion of yellow identifying stripes. It is fully stabilized against thermal degradation and the die build-up during extrusion is minimized. Furthermore, it has a highly covered pigment that gives a bright yellow stripe even when extruded as a thin layer on a black pipe. It also contains UV-stabilizer to ensure excellent weathering resistance.Borstar 3446 is recommended for identifying stripes of black pipe for natural gas produced from Borstar ME3440.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1183
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133