Material Notes:
Description: H 306 is a medium melt flow rate additivated homopolymer used for general purposes. It suitable for injection moulding and fiber extrusion. This product exhibits excellent processability, good melt stability and stiffness/impact strength balance. It also exhibits low odor and flavor transfer.Applications: Household; Sealed or flip-top closures; Staple fibers for rugs and blankets; Medium-toughness continuous filaments for yarns.Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.250 J/cm

@Temperature 23.0 °C
0.468 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
10 N; ASTM D1525