Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem MR 435 UV LMDPE Rotational Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem MR 435 UV LMDPE Rotational Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Water tanks; toys; automotive components. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.720 GPa
104 ksi
ASTM D790
Secant Modulus 1.80 GPa
261 ksi
1%; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Users viewing this material also viewed the following: