Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for extrusion and injection-blow molding. An antioxidant had been added to ensure thermal stability. Pro.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 110-1327 LMDPE Rotational Molding Resin Description: ICORENE 110-1327 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 110-3561 LMDPE Rotational Molding Resin Description: ICORENE 110-3561 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1327 LMDPE Rotational Molding Resin Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-3561 LMDPE Rotational Molding Resin Description: ICORENE 115-3561 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 190-3561 LMDPE Rotational Molding Resin Description: ICORENE 190-1332 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
Micropol Microlin ML20 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
Micropol Microlin ML21 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | base resin; ISO 1872-2/ISO 1183 |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2B |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2B |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Base Resin; ASTM D1505 |
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM-D1505 |
Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 705.MJ Molding, extrusion and compounding resin Escorene Ultra LD 705.MJ is a fraction melt index, 13.3 wt% vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles and compounds.Information provided by ExxonMobi.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | |
Dow Primacor® 4608 Ethylene Acrylic Acid (EAA) PRIMACOR® 4608 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating resin. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrat.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | compound; ISO 1183 |
Borealis LE6023 Polyethylene Modified Jacketing Compound LE6023 is a black flexible low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in.. |