Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Increased flex w/ living hinge propertiesCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packages, custom color matching, and processing additives.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Gardner Impact 10.2 J
7.52 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648