Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.00 GPa | 145 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-0803 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.00 GPa @Temperature 23.0 °C |
145 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE HJ-75 UV1 Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Flexural Modulus | >= 1.00 GPa | >= 145 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | |
Plastcom SLOVAMID 6 LI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol T100MK Polypropylene REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Flint Hills 23M2A Polypropylene Random Copolymer Features: High contact clarity, blush resistant, good impact, and stress resistant, good auto-clave stability, and low extractability. Product does not contain animal derived components.Application.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 3340H Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, HIGH IMPACT, GOOD EXTRUDABILITY APPLICATIONS: BLOW MOLDING, SHEET EXTRUSION FOR COSMETIC BOTTLES, SHEET FOR THERMOFORMING, CLOSURES, FILES |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178 |
MRC Polymers MAXTEL™ 600T15IMUV TPO, 15% Talc Filled • For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation pr.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-4161UV Thermoplastic Olefin Resin Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherabili.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ CA278A Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA278A is a thermoplastic polyolefin elastomer that is used for automotive interior partsFeatures: Good StiffnessHigh FlowGood MoldabilityGood Impact ResistanceLow Temper.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemi.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1692 Polypropylene High Impact Copolymer DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 5 mm/min, secant; ASTM D790 |
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 - 1.14 GPa | 145 - 165 ksi | tangent; ASTM D790 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | Tangent; ASTM D790A |
Bapolene® 3295 Polyethylene, Injection Grade Designed to offer improved cycle times and dimensional stability This product complies with US FDA 21CFR177.1250.Applications: Food containers and closures.Bapolene® and Bapolan® are registered t.. |
|||
Flexural Modulus | 1.00 GPa | 145 ksi | ASTM D790 |
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang. |