Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are oven handles, vent trim and control panels.
Physical Properties Metric English Comments
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Water Absorption 0.10 - 0.20 %
0.10 - 0.20 %
24 hours, 23°C
Linear Mold Shrinkage 0.0015 - 0.0040 cm/cm
0.0015 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 55
40 - 55
Tensile Strength, Ultimate 34.5 - 55.2 MPa
5000 - 8000 psi
Flexural Strength 68.9 - 124 MPa
10000 - 18000 psi
Flexural Modulus 11.0 - 13.8 GPa
1600 - 2000 ksi
Compressive Strength 124 - 152 MPa
18000 - 22000 psi
Izod Impact, Notched 1.07 - 3.20 J/cm
2.00 - 6.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C
425 - 500 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F