Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC A50-XHS Bulk molding compound

Category Polymer , Thermoset , Polyester, TS
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A50-XHS Bulk molding compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: BMC A50­XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in pre­weighted slugs. Due to the excellent flow and controlled reactivity, BMC A50­XHS is well suited for injection, transfer or compression molding. Typical applications are circuit breakers, lighting housings and structural parts.Information provided by Bulk Molding Compounds
Physical Properties Metric English Comments
Specific Gravity 1.79 - 1.99 g/cc
1.79 - 1.99 g/cc
molded
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength at Break 57.2 - 71.0 MPa
8300 - 10300 psi
Flexural Yield Strength 124 - 152 MPa
18000 - 22000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 116 - 143 MPa
16800 - 20800 psi
Izod Impact, Notched 5.34 - 6.41 J/cm
10.0 - 12.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 14.8 - 16.7 kV/mm
375 - 425 kV/in
Short Time
Arc Resistance >= 186 sec
>= 186 sec
Comparative Tracking Index <= 500 V
<= 500 V
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F
Users viewing this material also viewed the following: