Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound

Category Polymer , Thermoset , Polyester, TS
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC A50-XHS-U is well suited for injection, transfer or compression molding.Information provided by Bulk Molding Compounds
Physical Properties Metric English Comments
Specific Gravity 1.79 - 1.99 g/cc
1.79 - 1.99 g/cc
molded
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength at Break 57.2 - 71.0 MPa
8300 - 10300 psi
Flexural Yield Strength 124 - 152 MPa
18000 - 22000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 116 - 143 MPa
16800 - 20800 psi
Izod Impact, Notched 5.34 - 6.41 J/cm
10.0 - 12.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 14.8 - 16.7 kV/mm
375 - 425 kV/in
Short Time
Arc Resistance >= 186 sec
>= 186 sec
Comparative Tracking Index <= 500 V
<= 500 V
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F