Material Notes:
This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.70 %
0.70 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.5 %
1.5 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80

@Thickness 10.0 mm
80

@Thickness 0.394 in
ISO 2039-2
Tensile Strength, Yield 40.0 MPa
5800 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 178 °C
352 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 95.0 °C
203 °F
Long Term
150 °C
302 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 32.0 kV/mm
813 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.026

@Frequency 1e+6 Hz
0.026

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A
Users viewing this material also viewed the following: